Products
Cold Shrink Products
Silicone cold shrink tube
EPDM cold shrink tube
Cold shrink termination
Cold shrink joint
Cold shrink breakout
Others
Machine and Molding
Cold shrink machine
LSR injection machine
Expanding machine
Plastic core machine
Heat shrink machine
Molding
Others
Heat Shrink Products
Heat shrink tube
Heat shrink termination
Heat shrink joint
Others
Pre-mould Cable    Accessories
Pre-mould termination
Pre-mould joint
Others
Rubber Products
Silicone tube
LSR injection parts
Silicone moulding parts
Others
 
 

 

 

Pre-mould joint

8.7/15kV Silicone Rubber Pre-mould Joint

Voltage

1&3 core Pre-mould Joint

Suit for cable Section
(mm 2 )

Insulation OD
of Applicable Cables

8.7/15kV

JCP-10/3(1).1#

35

16.2¡«18.2

JCP-10/3(1).2#

50

17.8¡«19.6

JCP-10/3(1).3#

70

19.5¡«21.0

JCP-10/3(1).4#

95

20.5¡«22.5

JCP-10/3(1).5#

120

22.0¡«24.3

JCP-10/3(1).6#

150

23.5¡«25.8

JCP-10/3(1).7#

185

25.0¡«27.4

JCP-10/3(1).8#

240

27.0¡«29.5

JCP-10/3(1).9#

300

29.5¡«32.0

JCP-10/3(1).10#

400

32.5¡«34.8

JCP-10/3(1).11#

500

34.0¡«37.5

 

Test Standard for 8.7/15kV Pre-mould Joint

Sample test No.

Test Items

Requirements

Results

Remarks

8.7/15kV Silicone Rubber pre-mould Joint

JPC-10 3*185

AC withstand
voltage test

No flashover,No breakdown shall occur at 39kv for 5 min

No flashover,No breakdown shall occur at 39kv for 5 min

PASS

Partial discharge at testambient temperature

15kv,¡Ü10pc

2pc

PASS

Heating cycle voltage test in air

No flashover,No breakdown during 3 cycles at 95 ¡æ -100¡æ23kV

No flashover,No breakdown During 3 cycles at 95 ¡æ -100 ¡æ 23kV

PASS

Partial discharge test at 95 ¡æ -100¡æ

15kv,¡Ü10pc

2pc

PASS

Impulse withstand voltage test at 95 ¡æ -100¡æ

No flashover,
No Breakdown
95kV,¡À10 times

No flashover
No Breakdown 105kV, ¡À10 times

PASS

Dynamic short-circuit test

No visible deterioration at 80.1kA,not less than 10ms

No visible deterioration at 80.49 kA,67ms

PASS

AC withstand
voltage test under rain

No flashover No breakdown shall occur at 35kv 1min

No flashover No breakdown shall occur at 35kv 1min

PASS

 

 

 

                              £ü Home       £ü Products       £ü Online       £ü Contact       £ü E-Mail        £ü Map         £ü  Chinese      £ü  

         Tel:+86- 571-63817700   Fax: +86-571-63817700    Mobile: +86-13588233605
         Add: YuHang Zone, Hangzhou City, Zhejiang Province, China
         E-mail: betty@coldshrinktube.com

 

Copyright by Hangzhou BoChuang Rubber Technology Co., Ltd

All Rights Reserved